Evaluation Of Chemical Indexes To Predict The Dissolution Rate Of Amorphous Silicate Fibres In A Physiological Salt Solution

In order to predict the biosolubility of amorphous inorganic fibres through a chemical index, dissolution experiments were carried out of the amorphous silicate fibres in the RO-SiO2 system in a physiological salt solution at 40 deg C over 50h with shaking at 120 cycles/min. The correlation was analysed between the dissolution rate and each index such as carcinogenicity index (KI), nonbridging oxygen index (NBO), free energy of hydration, and molar ratio-weighted mean ionic radius of the alkaline earth ions as the glass network modifiers. The published indexes are based on the chemical composition of the fibre.

Author
M Ohsawa & Y Misu
Origin
Saint-Gobain, Chiba, Japan
Journal Title
Glass Sci Technol 76 6 2003 263-269
Sector
Glass Fibre
Class
GF 382

Request article (free for British Glass members)

Evaluation Of Chemical Indexes To Predict The Dissolution Rate Of Amorphous Silicate Fibres In A Physiological Salt Solution
Glass Sci Technol 76 6 2003 263-269
GF 382
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.