European Glass Recycling Trends - Impact On Raw Materials

The recycling of glass cullet has become of vital importance for environmental reasons and to the glass industry itself, but it also has an impact on glass raw material suppliers. This paper gives a comprehensive overall picture of the glass recycling trends in Europe over the past two decades and the impact that these trends have had on raw material supplies for glass production.