30 years ago, the recycling of used glass was introduced in Europe and has become a great success with a total average recycling rate of 59%, when considering the 17 European countries listed. 2002 showed another record year, with particularly strong growth in southern Europe. The recycling table for 2002 has been released by FEVE and is published in this article.