Estimation Of Handling Stresses In A 4 M Zerodur Blank With The Finite Element Method

It has been demonstrated that finite element analysis can be used to predict handling stresses, using as example a 4m Zerodur blank produced by spin casting.

Author
H Loch
Origin
Schott Glaswerke
Journal Title
Glastech Ber 1989 62 2 35-37
Sector
Glass Ceramics
Class
GC 38

Request article (free for British Glass members)

Estimation Of Handling Stresses In A 4 M Zerodur Blank With The Finite Element Method
Glastech Ber 1989 62 2 35-37
GC 38