Erosion And Damage By Hard Spherical Particles On Glass

Solid particle impact of hard spherical particles on glass is of fundamental interest because of the presence of a number of different impact regimes. Understanding the impact of spherical particles is also a step toward modeling the behaviour of rounded particles. This paper verifies theoretical models for the transitions between the different impact regimes and process parameters like erosion rate and surface roughness. The work also includes rounded particles. The transitions plotted in a so-called erosion map are validated with single-impact experiments. Data from erosion experiments are used to test the relations for the erosion rate and resulting surface roughness following from the models.

Author
P J Slikkerveer Et Al
Origin
Philips Research Labs, The Netherlands
Journal Title
J Am Ceram Soc 82 11 1999 3173-3178
Sector
Special Glass
Class
S 1754

Request article (free for British Glass members)

Erosion And Damage By Hard Spherical Particles On Glass
J Am Ceram Soc 82 11 1999 3173-3178
S 1754