Er3+ -Doped Tellurite Glasses For Enhancing A Solar Cell Photocurrent Through Photon Upconversion Upon 1500Nm Excitation

Trivalent erbium-doped tellurite glasses have been prepared and investigated with an aim to improve the efficiency of a Silicon (Si) solar cell through photon upconversion processes.

Author
K V Krishnaiah Et Al
Origin
Sri Venkateswara University, Tirupati, India
Journal Title
Materials Chemistry And Physics 199 2017 67-72