Equibiaxial Stress Effect On Fracture Strength Of Indented Soda-Lime Glass In Water Environment: An Examination For Dependence On Crack-Tip Blunting

The biaxial strengthening observed under restricted subcritical crack growth indicates that equibiaxial stress effects in a water environment are caused by the rounding of the initial crack tip.