Epsilon 5 - A New Spectrometer For Low-Level Detection Of Heavy Elements

For low level detection of heavy elements, a totally new energy-dispersive X-ray fluorescence (EDXRF) spectrometer, Epsilon 5, has been introduced by PANalytical. This spectrometer can detect elements from sodium to uranium in solid, pressed powder, granule, liquid, thin film and loose material samples. Measurements can be performed in a vacuum or helium atmosphere. In view of the growing environmental concern and stricter legislation, Epsilon 5 is designed to support applications in several fields, inducing land reclamation, fossil and secondary fuel usage, emissions monitoring, recycling, catalyst production and electronics and electrical appliance manufacture. Epsilon 5 excels at trace analysis of heavy elements, such as As, Pb, Cd and the lanthanides in concentrations from 100% down to sub-ppm levels. For more information contact: [email protected]

Author
Un-named
Origin
Unknown
Journal Title
Trans Ind Ceram Soc 63 2 2004 133
Sector
Special Glass
Class
S 2956

Request article (free for British Glass members)

Epsilon 5 - A New Spectrometer For Low-Level Detection Of Heavy Elements
Trans Ind Ceram Soc 63 2 2004 133
S 2956
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.