Epr Spectroscopy Of Cr(Iii) And Cr(V) Ions In Silica Xerogels Calcined At Various Temperatures

Chromium ions have been used as a paramagnetic spin label for the EPR spectroscopy investigation of the local structural changes of silica zerogels as a function of temperature during their calcination as well as during subsequent ageing.