Epr And Optical Absorption Spectra Of Vo2+ In Naf.B203 And Naf.Na20.B203 Glasses

The electron paramagnetic resonance and optical spectra of VO2+ in xNa2F2(100-x)B203, 5

Author
N C Biswas Et Al
Origin
Aligarh Muslim University, India
Journal Title
Phys Chem Glasses 37 2 1996 62-67
Sector
Special Glass
Class
S 976