Epma Study Of The Weathering Of Potash-Lime-Silciate Glasses

The deterioration of glass on exposure to atmosphere (weathering) varies with environmental parameters, time of exposure as well as with glass chemical composition. The analysis of 13-14th century glasses of stained windows in France and Germany identified 4 potash-lime-silica glass compositions. To investigate their weather weathering mechanisms and the impact of the environment on the conservation, glasses reproducing the original compositions were melted in the laboratory and their surfaces exposed in field for up to 12 months in different positions near the corresponding original stained glass windows. Furthermore, in order to ascertain the contribution of the glass composition to the weathering process, a laboratory test was developed to compare the durability of the four glasses.

Author
F Geotti-Bianchini Et Al
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 35 3 2005 49-61
Sector
Special Glass
Class
S 3240

Request article (free for British Glass members)

Epma Study Of The Weathering Of Potash-Lime-Silciate Glasses
Riv Staz Sper Vetro 35 3 2005 49-61
S 3240
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.