Epitaxial Crystallization Of Seeded Albite Glass

The role of solid-state epitaxy in the crystallisation of albite glass to glass-ceramic has been investigated.

Author
U Selvaraj Et Al
Origin
The Pennsylvania State University
Journal Title
J Am Ceram Soc 1991 74 6 1378-1381
Sector
Glass Ceramics
Class
GC 100

Request article (free for British Glass members)

Epitaxial Crystallization Of Seeded Albite Glass
J Am Ceram Soc 1991 74 6 1378-1381
GC 100