Environmentally-Friendly Glass Enamel

German-based Ceredec has recently announced the launch of a new environmentally-friendly enamel for automotive and arthitectural glass, after the successful completion of 6 months of field tests by its glass division. Today, highly opaque glass colours are available with environmental and technical advantages, some of which are: improved loading permits lower transmission of light; reduced VOCs allow wet-firing with less porosity; infrared curing installs a strong polymer network for greater film hardness; & warning label unnecessary because of non-toxic nature.

Author
Un-named
Origin
Unknown
Journal Title
Glass-Tech Int 3/96 24
Sector
News Items
Class
N 11

Request article (free for British Glass members)

Environmentally-Friendly Glass Enamel
Glass-Tech Int 3/96 24
N 11
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.