Environmentally Friendly, Abrasion Resistant Low Temperature Glass Coatings

With ever increasing regulations on the use of heavy metals and VOCs, more and more attention has been given to water borne, low temperature curing decorative coatings. Typically described as organic coatings, such materials offer the glass decorator a wide variety of colours. One issue with many such coatings however, has been the ease with which the surface can be scratched. This paper discusses the recent development of DuraSpray, an inorganic copolymer glass coating system for spraying applications. A discussion of processing parameters and general performance characteristics is included.

Author
S Garby & J Neely
Origin
Engelhard Corp & Neely Ind, Usa
Journal Title
Int Glass Review 3/2000 141, 143
Sector
Enamels
Class
E 55

Request article (free for British Glass members)

Environmentally Friendly, Abrasion Resistant Low Temperature Glass Coatings
Int Glass Review 3/2000 141, 143
E 55
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.