Environmental And Health Issues In The Glass Industry

Developments in control technology which have been implemented to satisfy the tightening environmental regulations are reviewed.

Author
G Geiger
Origin
Unknown
Journal Title
Ceramic Bulletin 1992 71 2 193-199