Environmental Analysis For Identifying Challenges To Recover Used Reinforced Refractories In Industrial Furnaces

Reinforced refractories have been demonstrated to be economically and technically useful in industrial furnaces to improve energy efficiency. Nevertheless, there is a lack of knowledge from the environmental point of view in which the end-of-life of these materials was analysed from a life cycle perspective. This research examines the use of the Life Cycle Assessment (LCA) methodology to evaluate the environmental impact of alumina/ZrO2 and MgO/ZrO2 as reinforced refractories, considering the manufacturing and two different end-of-life scenarios, disposal in landfills and recycling. The results indicated that the environmental performance of these reinforced refractories can be improved by means of promoting the reuse or recycling of the materials and reducing the amount of landfill waste within an integrated waste management system. Greater environmental benefits were obtained when the recycling efficiency was increased and the transport distance was decreased, especially in the case of alumina/ZrO2. The research demonstrated that it was more sensible to use recycling. Consequently, efforts to consider these environmental results should be undertaken by the industrial sector to promote material recovery. In this sense, a matrix of additional actions is proposed to reduce the overall environmental impact of the system further.

Author
G Ferreira Et Al
Origin
Unknown
Journal Title
J Cleaner Production 88 1 February 2015 242-253
Sector
Refractories
Class
R 841

Request article (free for British Glass members)

Environmental Analysis For Identifying Challenges To Recover Used Reinforced Refractories In Industrial Furnaces
J Cleaner Production 88 1 February 2015 242-253
R 841
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.