Entropy Diagram For The Glass Quenching Cycle

A method for analysis of entropy diagrams plotted on T-S and H-S coordinates is proposed. The method can be used in laboratory and industiral research for quenching cycle efficiency analysis in the production of thin and ultrathin glasses of various compositions.