Enhancing In Vitro Bioactivity Of Melt-Derived 45S5 Bioglass

45S5 Bioglass is a frequently applied Type A bioactive material, capable of forming an inherent bond to bone and soft tissue. Currently, applied melt-derived bioactive glass powders exhibit particle sizes between a few to several hundred micrometers. Recent studies on nanometer-sized bioactive glasses (nBGs), produced by bottom-up methods like sol-gel processing or flame spray pyrolysis, have indicated their great potential for several biomedical applications. In this study, the feasibility of top-down processing starting from bulk 45S5 BG by wet comminution in a stirred media mill was investigated.

Author
S Romeis Et Al
Origin
Inst Particle Technol, University Erlangen-Nuremberg, Germany
Journal Title
Jacs 97 1 2014 150-156
Sector
Special Glass
Class
S 4146

Request article (free for British Glass members)

Enhancing In Vitro Bioactivity Of Melt-Derived 45S5 Bioglass
Jacs 97 1 2014 150-156
S 4146
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 15 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.