Enhanced Near-Infrared To Green Upconversion From Er3+ Doped Oxyfluoride Glass And Glass Ceramics Containing Bagdf5 Nanocrystals

In this work, the effect of glass composition, as well as ceramization on visible and near-infrared (NIR) luminescence properties along with tehir decay dynamics of Er3+ ions has been compared considering two different oxyfluoride glasses yielding BaF2 and BaGdF5 nanocrystals.

Author
K Biswas Et Al
Origin
Csir, Kolkata, India
Journal Title
Int J Appl Glass Sci 8 2017 204-215
Sector
Glass Ceramics
Class
GC 895

Request article (free for British Glass members)

Enhanced Near-Infrared To Green Upconversion From Er3+ Doped Oxyfluoride Glass And Glass Ceramics Containing Bagdf5 Nanocrystals
Int J Appl Glass Sci 8 2017 204-215
GC 895