Enhanced Electrocaloric Effect In Glass-Added 0.94Bio.5Nao.5Tio3-O.O6Batio3 Ceramics

In this study, 3BaO-3TiO2-B2O3 (BTBO) glass-added 0.94BiO.5NaO.5TiO3-O.O6BaTiO3 (BNT-BT) ferro-electric ceramics were synthesized using a conventional solid-state reaction methodology. The electrocaloric effect on glass-added ceramics was calculated using Maxwell relations. The maximum adiabatic temperature changes of 0.21, 0.25, and 0.14 K were obtained at 40 kV/cm for 2, 4, and 6% glass addition which are significantly higher than those of the pure sample (0.008 K) under study. The results reveal that glass addition up to 4% resulted in enhanced electrocaloric response. Further, the effect of glass addition on the dielectric properties was investigated. The dielectric constant decreases with glass addition compared with pure TNT-BT at 303 K.

Author
K S Srikanth Et Al
Origin
Indian Inst Technology, Mandi, Kamand, India
Journal Title
J Aust Ceram Soc 53 2017 523-529
Sector
Special Glass
Class
S 4419

Request article (free for British Glass members)

Enhanced Electrocaloric Effect In Glass-Added 0.94Bio.5Nao.5Tio3-O.O6Batio3 Ceramics
J Aust Ceram Soc 53 2017 523-529
S 4419
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.