Energy-Saving Windows Getting Smarter, Cheaper

The US Department of Energy's National Renewable Energy Laboratory (NREL) scientists are developing an insulating window film that "Preserves the view while increasing occupants' comfort and saving energy," according to an NREL press release. The film incorporates nanometer- to micrometer-sized vacuum capsules that can be applied like conventional low-e window tinting films. "Early estimates indicate that a millimeter-thick layer results in clear insulation with values equivalent to R-20, which is equal to standard wall insulations," the release says, adding that: "The window film could reduce building energy use by as much as 33%, resulting in a payback period of less than a year while saving energy and reducing greenhouse gas emissions."

Author
Un-named
Origin
Unknown
Journal Title
Am Ceram Soc Bull 93 1 2014 21
Sector
Flat glass
Class
F 3562

Request article (free for British Glass members)

Energy-Saving Windows Getting Smarter, Cheaper
Am Ceram Soc Bull 93 1 2014 21
F 3562
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.