Energy And Entropy Of Crystals, Glasses And Melts

The molar entropy, S, and enthalpy (energy), H, of crystals, glasses and melts of the same one-component systems have been suitably visualised including the transformation from the melt into a glass or crystallisation. For the temperature T>OK the enthalpy and entropy of the glass are larger as compared to the stable crystal. The S and H functions of glasses correspond to a simple continuation of these functions from the molten state to lower temperatures. Crystallisation occurs as a spontaneous process under production of entropy. Extrapolating the entropy of the molten and crystalline sates from the melting range to lower temperatures, which is the basic of "Kauzmann's paradox", is ambiguous and misleading, as the extrapolated data deviate considerably from the experimental temperature dependencies of S of glasses and crystals.

Author
H Hoffmann
Origin
Technische University Berlin, Germany
Journal Title
Glass Sci Technol 78 5 2005 218-229
Sector
Special Glass
Class
S 3029

Request article (free for British Glass members)

Energy And Entropy Of Crystals, Glasses And Melts
Glass Sci Technol 78 5 2005 218-229
S 3029
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.