Energy Analysis Of The Oxygen Combustion In A Glass Furnace (In Italian)

Glass furnaces using air as a combustant and those using oxy-fuel are compared in this article.

Author
R Dall'Igna
Origin
Unknown
Journal Title
Rivista Della Staz Sper Vetro 22 5 1992 239-250