By means of its advanced services program, Emhart Glass has helped glassmakers worldwide address specific container production issues. The company now presents the next step - the Pack+ a combination of advanced services programs, proprietary technologies, and an experienced staff of production specialists. By applying Six Sigma methodologies, Pack+ finds and resolves root causes of problems.