Emhart Glass: Ais - Pneumatic Is Machinery At Its Best

The times when container market demands could be predicted are gone. Therefore, the key requirements and driving forces for new IS machines are performance in conjunction with quality and flexibility. The Advanced Individual Section machine (AIS) is, nowadays, recognised by the glass industry as the superior performer amongst pneumatically driven IS machines. This article describes the AIS machine in more detail - providing a very cost effective way to benefit from familiar technology, with the option of servo electric take-out, invert and the two-axes servo controlled FlexPusher.

Author
Un-named
Origin
Unknown
Journal Title
Gmpa 3/07 68-70
Sector
Container glass
Class
C 3362

Request article (free for British Glass members)

Emhart Glass: Ais - Pneumatic Is Machinery At Its Best
Gmpa 3/07 68-70
C 3362
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.