Elimination Of Heavy Metals From Leachates By Membrane Electrolysis

The elimination of heavy metals from bioleaching process waters by electrolysis was studied in the anode/cathode region of a membrane electrolysis cell at densities of 5-20mA/cm2.The leaching waters containing a wide range of dissolved heavy metals, were high in sulfate, & had pH values of approximately 3. In preliminary tests using a rotating disc electrode, the current density-potential curve (CPK) was recorded at a rotation velocity of 0, 1000 & 2000 rpm & a scan rate of 10 mV/s in order to collect information on the influence of transport processes taking place at the electrodes. Electrochemical deposition-dissolution processes at the cathode is strongly dependent on hydrodynamics. Examining anodic oxidation of dissolved Mn(II) indicated that manganese dioxide which formed adhered well to the electrode surface but in the cathodic return run was reduced.

Author
R Fischer Et Al
Origin
Technische Universitat Dresden, Germany
Journal Title
Eng Life Sci 4 5 2004 438-444
Sector
Special Glass
Class
S 2894

Request article (free for British Glass members)

Elimination Of Heavy Metals From Leachates By Membrane Electrolysis
Eng Life Sci 4 5 2004 438-444
S 2894
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.