Eliminating Rat Holes In Furnace Silica Crowns

The Bulgarian company Lubisol Engineering Co. has developed a method for eliminating loose joints in silica crowns. Known as Zero Joint technology, it is said to give a success rate close to 100% in overcoming the problems of alkaline corrosion and rat hole formation.