Elemental Minerals' Sintoukola Potash Deposit

Elemental Resources uses software packages to improve accuracy of resource estimation for its Sintoukola potash deposit. In this paper the authors outline how the gridding seam method is appropriate for deposit modelling.

Author
Dr A Scogings & Dr S Dorling
Origin
Csa Global Pty Ltd
Journal Title
Industrial Minerals August 2014 44-48
Sector
General
Class
G 4256