Elemental Analysis Of Small Glass Fragments In Forensic Science

The evidential value of small glass particles has been recognised for quite some time. While physical properties such as RI & density offer some discrimination of samples, they offer little in the way of classification of glass product type. Further, with improved glass manufacturing process, the range of physical properties seen in modern glass samples is decreasing. Many have advocated the use of elemental analysis for the purpose of forensic glass analysis. Various instrumental techniques have been employed, including flameless atomic absorption spectrometry, inductively coupled plasma atomic emission spectrometry, & energy dispersive X-ray fluorescence spectrometry. These more commonly employed methods are discussed with regard to the application to forensic glass analysis. Advantages & disadvantages of each technique are highlighted.

Author
J A Buscaglia
Origin
John Jay College Criminal Justice, New York, Usa
Journal Title
Analytica Chimica Acta 288 2004 17-24
Sector
Special Glass
Class
S 2863

Request article (free for British Glass members)

Elemental Analysis Of Small Glass Fragments In Forensic Science
Analytica Chimica Acta 288 2004 17-24
S 2863