Elemental Analysis Of Glass And Glass Ceramics With The Scanning Electron Microscope

An x-ray energy dispersive system consisting of lithium drifted silicon detector and a computer as a multichannel analyser is used to determine the elemental composition of glass, glass ceramic and other materials with the scanning electron microscope. In general all elements of atomic number 11 (sodium) or higher can be detected in selected microareas when present in amounts from 0.25 to 0.5% or higher. Resolution of the analysis site to volumes as small as approximately 2 um3 can be attained.

Author
Ej Korda Et Al
Origin
Unknown
Journal Title
American Ceramic Society Bulletin 52 3 1973 279-284
Sector
Primary Papers
Class
PP 1290

Request article (free for British Glass members)

Elemental Analysis Of Glass And Glass Ceramics With The Scanning Electron Microscope
American Ceramic Society Bulletin 52 3 1973 279-284
PP 1290
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.