Elemental Analysis And The Discrimination Of Sheet Glass Samples

Several analytical techniques have been employed to measure the concentrations of 22 elements in 15 colourless sheet glass samples of refractive index 1.5160-1.5161. The elemental data have been examined inorder to identify the best variables to discriminate the glass samples. The concentrations of Mn, Fe, Mg, Sr, and Ba in 232 samples of sheet glass have been determined using inductively coupled plasma-atomic emission spectrometry. The samples were selected as representative of 10 narrow ranges of r.i. within the region 1.5150-1.5210.

Author
D A Hickman
Origin
Metropolitan Police Forensic Science Lab
Journal Title
Forensic Science Journal 23 1983 213-223
Sector
Special Glass
Class
S 5071

Request article (free for British Glass members)

Elemental Analysis And The Discrimination Of Sheet Glass Samples
Forensic Science Journal 23 1983 213-223
S 5071
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.