Electrostatic Precipitator Dust - Waste Product Or Useful Batch Material?

A look at two operating systems that incorporate EP dust in the glassmaking process.

Author
D T Boothe Et Al
Origin
D Boothe & Co Inc, Usa
Journal Title
Glass Industry 75 5 1994 20, 23-25, 29