The Electronic Structure And Optical Properties Of Oxide Glasses I. Sio2, Na2O,: Sio2 And Na2O:Sio2

A combined spectroscopic and theoretical study of the above glasses has been carried out. (file copy with Jon Bentley)

Author
E Ellis & D W Johnson
Origin
Pilkington Bros
Journal Title
Philosophical Magazine B, 1979, 40 2 105-124