Electronic Spectral Study Of Co(Ii) Complexes In Potassium Borate Glasses With Low Alkali Oxide Contents

Glasses containing 5-11 mol% potassium oxide have been investigated.

Author
K Kojima, J Matsuda, T Kimura
Origin
Ritsumeikan University, Murata Mfg Co. Ltd
Journal Title
Physics And Chemistry Of Glasses 1988 29 4 154-156