Electron Microscopic Investigations Of Electrochemically Induced Mullite Crystallisation In A Glassy Matrix

The electrochemically induced nucleation and crystallisation in a glass with t he basic composition (mol%) 52.6 SiO2 - 18.7 Al2O3 - 14.3 MgO - 7,8TiO2 - 4.7 B2O3 - 2.0 CaO leads to the formation of of oriented mullite crystals. Electron microscopy techniques (energydispersive X-ray microanalysis and electron backscatter diffraction) were used to analyse the composition and the orientation of the crystals in the glassy matrix. The mean composition of the mullite crystals matches the formula (formula). The electron backscatter diffraction patten is consistent with data from the literature that needle-like mullite crystals are fast growing parallel to the crystallographic c-axis [001]. The composition of the melt grown mullite crystals does not depend on the melting temperature in the range between 1230C and 1350C.

Author
R. Carl Et Al
Origin
Universitat Jena, Jena, Germany
Journal Title
Advanced Materials Research Vols 39-40 (2008) 387-390
Sector
Special Glass
Class
S 3417

Request article (free for British Glass members)

Electron Microscopic Investigations Of Electrochemically Induced Mullite Crystallisation In A Glassy Matrix
Advanced Materials Research Vols 39-40 (2008) 387-390
S 3417
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.