Electron Microprobe Data Collection And Processing System For The Microvolume Analysis Of Glass

Sample surface heating has been reduced by using a more sensitive energy dispersive x-ray detector, and a digital scanning technique which allows the acquisition of quantitative x-ray data by sampling each point on the surface both more frequently and for much shorter periods of time