Electron Beam Melted Molybdenum Applied In Glass Melting Electrodes

Electron beam melted molybdenum electrodes have been used successfully in glass melting furnaces for over 30 years. They are used in the form of rod-type electrodes with different diameters and in the form of block electrodes and as top electrodes in fully electrically heated glass melting furnaces and in cases of additional electricity heating in gas heated furnaces. As a result of the newly developed electrodes with a reduced proportion of gas forming components, molybdenum electrodes are available that are suitable for all areas of melting technology.

Author
C Michelsen Et Al
Origin
Csm Industries Inc, Usa
Journal Title
Int Glass Review (Online) 2 2002
Sector
General
Class
G 3131

Request article (free for British Glass members)

Electron Beam Melted Molybdenum Applied In Glass Melting Electrodes
Int Glass Review (Online) 2 2002
G 3131
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.