Electrochromic Films Via Sol-Gel Method

This paper provides an overview of what has been achieved in the field of chromogenic materials (anodic or cathodic electrochromic coatings and ion storage electrodes) used in electrochromic (EC) devices. It also looks at future developments in ths field.