Electrochemical surface treatment of a glass by lead-copper melts was investigated and the contents of the anode elements in the glass were determined. It was shown that the glass colour changes as a function of the treatment time. The variation in the content of lead and copper in the glass was established also as a function of the treatment duration. Based on the data obtained, a technology for the production of new materials from glass can be developed. The surface of these materials is coloured by the ions of lead and copper.

Author
R D Sytnik Et Al
Origin
Kharkov Polytechnic Inst, Ukraine
Journal Title
Glastech Ber Glass Sci Technol 74 6 2001 161-165
Sector
Special Glass
Class
S 2217

Request article (free for British Glass members)

Electrochemical Surface Treatment Of Glass By A Lead-Copper Melt
Glastech Ber Glass Sci Technol 74 6 2001 161-165
S 2217
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.