Electrically Controlled Light Transmission Glazing

The advent of new liquid crystal technology and its application to variable transmission glazing are described.

Author
P Van Konynenburg, R Wipfler, B Kennedy
Origin
Taliq Corporation
Journal Title
Glass Production Technology International 1990 170-174
Sector
Flat glass
Class
F 224