Electrical Resistivity Of Glass In Furnaces With Coaxially Mounted Cylindrical Electrodes

A novel hexagonal electric furnace for the production of cullet, rod or tubing made from high melting point glasses has been designed. The furnace is operated on the closed-top principle and is capable of producing 2.5 - 2.8 tonnes/m2/day. Compared with the De Bussy-type furnace, there is no need for a water-jacket or special water cooling system. Empirical formulae derived from cold model studies have been developed for calculating the resistances.

Author
K M Tatevosyan And Yu N Petrosyan
Origin
Glass And Ceramics 44 1-2 January-February 1987 14-16
Journal Title
Refer to Origin
Sector
Special Glass
Class
S 5015

Request article (free for British Glass members)

Electrical Resistivity Of Glass In Furnaces With Coaxially Mounted Cylindrical Electrodes
Refer to Origin
S 5015
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.