Electrical Properties Of Superionic Conducting Glasses In The Pseudobinary System Cui-Cu2Moo4

Cu+-ion-conducting glasses were prepared in the pseudobinary system CuI-Cu2MoO4. The electronic conductivity was measured by the Wagner polarisation method and indicates that the number of Cu+ ions in these glasses is 0.9996 and larger.