A scale-up rule is developed to estimate the resistance for each circuit of a projected glass melter. Given all the internal sizes and contours including shapes of the electrodes as well as the power and power ratios and the resistivity of the molten glass for the proposed melter, this rule permits calculating the voltage and current for each of its circuits. Single-phase circuit-interactions, distributions of equipotential surfaces and lines of current and some safety considerations are discussed and illustrated for a multiplicity of electrodes and single-phase power supplies by using two-dimensional, isothermal, salt water models of electric melters.

Author
P F Spremulli
Origin
Corning, Usa
Journal Title
Glastech Ber Glass Sci Technol 69 4 1996 83-94
Sector
General
Class
G 1441

Request article (free for British Glass members)

Electrical Modelling And Scale-Up Rules For Glass Melters
Glastech Ber Glass Sci Technol 69 4 1996 83-94
G 1441
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.