Electrical Conductivity Of Silver Vanadium Tellurite Glasses

The electrical properties of glasses have been studied extensively for several years, because of their potential use in solid-state devices. Most published data on mixed electronic-ionic conduction in glasses have been interpreted in terms of an ion-polaron correlation effect, which results from the coulombic attraction between oppositely charged carriers. To have a clear understanding of the conduction mechanism, one must establish the structural basis of transport properties of such mixed conductors. In this paper a study of the electrical conductivity of the 0.5[xAg20.(1-x)V205]-0.5Te02 glassy system and an attempt to explain the results in view of the structural information obtained from X-ray photoelectron spectroscopy (XPS) is given.

Author
H M M Moawad Et Al
Origin
Lehigh University, Usa
Journal Title
J Am Ceram Soc 85 11 2002 2655-2659
Sector
Special Glass
Class
S 2458

Request article (free for British Glass members)

Electrical Conductivity Of Silver Vanadium Tellurite Glasses
J Am Ceram Soc 85 11 2002 2655-2659
S 2458
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.