Electrical Conductivity Of Glasses And Glass-Ceramics In The Li2O-Cdo-Al2O3-Sio2 System

Electrical conductivity measurements are carried out at ambient temperature after controlled nucleation and crystalisation treatments and the relationship between conductivity and crystalline phase composition is discussed.

Author
J Rincon
Origin
Instituto De Ceramica Y Vidrio, Madrid
Journal Title
Bol Soc Esp Ceram Vidrio 1991 30 6 504 - 507