An investigation of the electrical conduction mechanism in Ge20BixSe70-xTe10(x=7,9,11,13) thin films in the temperature range of 300-425K with both symmetric and asymmetric electrodes is reported. The results were interpreted in terms of a Poole-Frenkel type of conduction mechanism operating over the entire range of temperature and field strength.