Electrical Conduction By Fast Ion Transport In Molten (Agi)X(Agpo3)1-X Glasses

The electrical conductivity of molten silver-iodide phosphate glasses has ben measured in a range of frequencies and the temperature range from near their respective glass transition temperatures to 770 K in both the normal and supercooled states.