Electrical Characteristics Of Horizontal Glass Melting Furnaces And Delivery Systems

Leakage currents and their low resistance paths through refractories from the interior of glass melting furnaces to the binding steel are discussed. By definition, a ground current flows from an electrode, through the intervening glass to ground through grounding conductors. All melters have leakage currents and may have ground currents. Current and voltage characteristics and phasor diagrams have been analysed for some circuits that can be used in horizontal melters.

Author
P F Spremulli
Origin
Corning Inc, Usa
Journal Title
Glastech Ber Glass Sci Technol 69 7 1996 193-203
Sector
Special Glass
Class
S 1055

Request article (free for British Glass members)

Electrical Characteristics Of Horizontal Glass Melting Furnaces And Delivery Systems
Glastech Ber Glass Sci Technol 69 7 1996 193-203
S 1055
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.