Electrical And Structural Characteristics Of Copper Oxide (I) Containing Lithium Phosphate Glasses

Oxide glasses containing transition metal ions are of enhanced interest because of their applications in information storage, electrical and optical switching devices. The aim of this work is to design, fabricate and characterise semiconducting glasses containing copper oxide. In such glasses, copper is expected to provide mixed conduction with contributions from copper ions as well as from polarons to ionic and electronic conductivity, respectively.

Author
C Mugoni Et Al
Origin
University Of Modena & Reggio Emilia, Italy
Journal Title
J Aust Ceram Soc 47 2 2011 42-43
Sector
Special Glass
Class
S 3730

Request article (free for British Glass members)

Electrical And Structural Characteristics Of Copper Oxide (I) Containing Lithium Phosphate Glasses
J Aust Ceram Soc 47 2 2011 42-43
S 3730
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.