[Electric Melting] Properties Of A Protective Layer On Mo Electrodes

As molybdenum electrodes corrode at high temperatures, they require robust protection. In this article the author discusses the properties of a protective layer during cathodic protection of the molybdenum electrode, with images to illustrate coated electrodes in various states.